ISO Standards for Materials Testing » ISO 11897 Thermoplastic Flexible Film Packaging, Tear Propagation Edge Folds

ISO 11897:1999 Tear Propagation on Edge Fold of Thin Film

ISO 11897 is a test method to determine tear propagation and tear resistance properties on edge fold of sacks made from thermoplastic flexible film.

Specimens are cut in a trapezoidal shape with the edge fold position in the center.  Then, a 25mm incision is cut along the edge fold.  The specimen is pulled apart, until failure, at a constant rate of displacement. The force and displacement are recorded as the tear propagates through the entire edge fold of the specimen, and is used to calculate the resistance to tear propagation of the material.

The challenges of testing to this standard are:

  • Specimen gripping
  • Reporting calculations in compliance with the standard

Instron's Solution:

  • Specimen gripping - In order to mitigate the influence of the grips on the specimen, rubber coated faces are commonly recommended for use with either side acting manual or pneumatic grips.
  • Reporting calculations in compliance with the standard - Instron's Bluehill® Universal testing software allows users to input specimen details, set the desired test control, automatically calculate the desired results and statistics, and produce a test report all in accordance with the standard.

It is important to review ISO 11897:1999 in order to fully understand the test setup, procedure, and results requirements.

Literature

2712-04x Series Pneumatic Side Action Grips Data Sheet

Instron’s 2712‑04x Series pneumatic grips deliver reliable, self‑centering gripping for a wide range of materials with options from 1 to 10 kN. Designed for safety and efficiency, they feature tool‑free jaw face changes, adjustable air‑controlled gripping force, robust enclosed mechanisms, and ergonomic components that improve alignment, usability, and operator protection.

  • Products
  • 03/22/2022
  • 1.13 MB

2710 Series Screw Side Action Grips

Screw side‑action grips offer a straightforward and reliable way to secure test specimens across a wide range of applications. The dual‑acting design of the 2710‑100 series allows the jaw faces to adjust easily for different specimen thicknesses, keeping the tensile load path centered within the grip body. These grips support a variety of interchangeable jaw faces in multiple sizes and surface types, including smooth ground, rubber‑coated, serrated, line‑contact, and specialty coated options. A convenient snap‑on attachment system makes swapping jaw faces fast and hassle‑free, adding flexibility for diverse testing needs.

  • Products
  • 06/28/2017
  • 1.29 MB

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.

  • Products
  • 02/10/2020
  • 4.15 MB

3400 Series Universal Testing Systems Brochure

Instron 3400 Series universal testing systems for tensile, compression, bend, and other material property tests.

  • Products
  • 06/27/2022
  • 2.69 MB