ISO Standards for Materials Testing » Tensile Strength of Basalt Fiber Reinforced Plastic (BFRP) Rebar

Tensile Strength of Basalt Fiber Reinforced Plastic (BFRP) Rebar

Basalt is a natural hard, dense, dark brown to black volcanic igneous rock. It is the most common rock type in the earth’s crust. Its origins are at a depth of hundreds of kilometers beneath the earth and reach the surface as molten magma. The volcanic rock in general is widely available in various regions of the world. Basalt finds its way into wide application in industry as abrasion, wear and chemical resistant materials. In recent years a new type of FRP composite material has been developed called Basalt Fiber Reinforced Plastic (BFRP) material. The characteristics of this material have various beneficial features such as high strength-to-weight ratio, lower specific weight and excellent corrosion and fatigue resistance. Nowadays this material is finding their way to more novel applications in relation to civil engineering structures. The use of Basalt in rebar applications, the physical testing results have shown to have ultimate tensile strength which is up to 4 times higher than the tensile strength of conventional steel rebar.

For the tensile testing of BFRP composite rebar, it is important that the specimens are prepared with tabbed ends in order to guarantee an adequate clamping of the specimen. This ensures that specimen breaks occur within the gauge length and not within the jaw face. For this test, we recommend the use of the model 5985 floor test system, 250kN capacity for tensile testing applications.

Before starting the test, the specimen is measured, then placed into 250kN hydraulic wedge grips. During the gripping process of the specimen, specimen protect feature is selected that allows you to set a load threshold that won't be exceeded until the test is started. A strain gauged clip-on extensometer; 25mm gauge length with 10% travel capability is attached to the specimen.

Bluehill 3 test software package is used to input specimen parameters, set the desired test speed control, automatically calculate the desired results and statistics, and finally produce a test report.

Literature

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.

  • Products
  • 02/10/2020
  • 4.15 MB

Bluehill Universal Brochure

Bluehill Universal is Instron’s advanced materials testing software, designed for intuitive touch interaction and streamlined workflows. It offers pre-loaded test methods, QuickTest for rapid setup, enhanced data exporting, and Instron Connect for direct service communication. Users of Bluehill 2 and Bluehill 3 can easily upgrade to the latest version for improved performance and usability.

  • Products
  • 02/26/2017
  • 3.76 MB

2630 Series Strain Gauge Extensometers

The 2630-100 series of extensometers offers speed of attachment and ease-of-use. The light-weight, rugged cross-brace design eliminates errors caused by physical distortion, while built-in protection ensures that damage is not caused by over-extension.

  • Products
  • 06/03/2013
  • 551.73 KB